Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shin-Etsu Silicones SV-55002U High Strength Silicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones SV-55002U High Strength Silicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SV55002U is one of a series of silicone bases Type of HCR designed for applications requiring high strength. Product Features: Excellent mechanical properties.Typical Applications: Molding and Extrusion applications for a wide range of productsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
DCBP Cure
1.13 g/cc
1.13 g/cc
DBPH Cure
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
DBPH Cure
50
50
DCBP Cure
Tensile Strength at Break 9.31 MPa
1350 psi
DCBP Cure
9.65 MPa
1400 psi
DBPH Cure
Elongation at Break 660 %
660 %
DCBP Cure
660 %
660 %
DBPH Cure
Tear Strength 33.3 kN/m
190 pli
Die B; DCBP Cure
33.3 kN/m
190 pli
Die B; DBPH Cure
Compression Set 10 %

@Temperature 100 °C,
Time 252000 sec
10 %

@Temperature 212 °F,
Time 70.0 hour
DCBP Cure
Processing Properties Metric English Comments
Cure Time 10.0 min
0.167 hour
240 min

@Temperature 200 °C
4.00 hour

@Temperature 392 °F
Post
Descriptive Properties Value Comments
Cure Agent DBPH
DCBP
Cure Type Press Cure