Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zoltek Panex 35® Stitch-Bonded Uni-Directional Carbon Fiber Fabrics

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Zoltek
Trade Name Panex 35®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zoltek Panex 35® Stitch-Bonded Uni-Directional Carbon Fiber Fabrics.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Stitch-Bonded Uni-Directional Carbon Fiber FabricsApplications include: Infrastructure, Body Panels, Wind Blade Spars
Physical Properties Metric English Comments
Thickness 400 microns
15.7 mil
Dry Thickness
440 microns
17.3 mil
Dry Thickness
570 microns
22.4 mil
Dry Thickness
760 microns
29.9 mil
Dry Thickness
900 microns
35.4 mil
Dry Thickness
1190 microns
46.9 mil
Dry Thickness
1250 microns
49.2 mil
Dry Thickness
Component Elements Properties Metric English Comments
Carbon, C 95 %
95 %
Descriptive Properties Value Comments
Areal Weights, g/m2 150
200
300
500
600
860
900
Roll Length, m 100
185
30
50
Roll Width, cm 120
30
60
Stitch Pattern, Glass Tricot