Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer

Category Polymer , Thermoplastic , Fluoropolymer , FEP
Manufacturer Shandong Dongyue Shenzhou New Material Co
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coefficient of friction, enabling thermoplastic processing methods.Main Applications:Extrusion processed for generic type resin, mainly used for wire insulation layer, tubes, film, and so on.Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
Volatiles <= 0.10 %
<= 0.10 %
Melt Flow 4.1 - 8.0 g/10 min
4.1 - 8.0 g/10 min
A
8.1 - 12 g/10 min
8.1 - 12 g/10 min
B
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 21.0 MPa
>= 3050 psi
Elongation at Break >= 300 %
>= 300 %
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Electrical Properties Metric English Comments
Dielectric Constant <= 2.15

@Frequency 1.00e+6 Hz
<= 2.15

@Frequency 1.00e+6 Hz
Dissipation Factor <= 0.00070

@Frequency 1.00e+6 Hz
<= 0.00070

@Frequency 1.00e+6 Hz
Descriptive Properties Value Comments
Appearance Translucent particles, without impurities such as metal debris and sand, containing visible black particles percentage point less than 2%