Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Seals Eastern 5484 Nitrile Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Seals Eastern, Inc
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Seals Eastern 5484 Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Low temperature service NitrileInformation provided by Seals Eastern, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D297, 15
Mechanical Properties Metric English Comments
Hardness, Shore A >= 75
>= 75
ASTM D2240, Type A
85
85
AVG; ASTM D2240, Type A
85
<br>@Temperature 100 °C,<br> Time 252000 sec
85
<br>@Temperature 212 °F,<br> Time 70.0 hour
After Dry Heat Aging; ASTM D865
Tensile Strength at Break >= 6.76 MPa
>= 980 psi
ASTM D412 Method A
12.39 MPa
1797 psi
AVG; ASTM D412 Method A
10.90 MPa
<br>@Temperature 100 °C,<br> Time 252000 sec
1581 psi
<br>@Temperature 212 °F,<br> Time 70.0 hour
ASTM D865
Tensile Strength, Yield >= 1.98 MPa
>= 287 psi
Stress at Elongation M50; ASTM D412 Method A
2.61 MPa
378 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 3.70 MPa
>= 536 psi
Stress at Elongation M100; ASTM D412 Method A
4.52 MPa
655 psi
AVG Stress at Elongation M50; ASTM D412 Method A
7.626 MPa
1106 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 68 %
>= 68 %
ASTM D412 Method A
163 %
163 %
AVG; ASTM D412 Method A
161.4 %
<br>@Temperature 100 °C,<br> Time 252000 sec
161.4 %
<br>@Temperature 212 °F,<br> Time 70.0 hour
ASTM D865
Modulus of Elasticity 0.01498 GPa
2.172 ksi
ASTM D412 Method A
Shear Modulus 0.00499 GPa
0.724 ksi
ASTM D412 Method A
Secant Modulus 0.01408 GPa
2.042 ksi
ASTM D412 Method A
Compression Set 10 %
<br>@Temperature 100 °C,<br> Time 79200 sec
10 %
<br>@Temperature 212 °F,<br> Time 22.0 hour
ASTM D395, Test B
19 %
<br>@Temperature 100 °C,<br> Time 252000 sec
19 %
<br>@Temperature 212 °F,<br> Time 70.0 hour
ASTM D395, Test B
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -29.4 °C
-21.0 °F
ASTM D1329
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
ASTM D395, Test B
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 39
Copyright © lookpolymers.com All Rights Reserved