Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR Suprex Clay Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0Suprex Clay60.0Coumarone-Indene Resin20.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
Mooney Viscosity 13

@Temperature 121 °C
13

@Temperature 250 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
Tensile Strength, Yield 15.2 MPa
2200 psi
Elongation at Yield 725 %
725 %
100% Modulus 0.00241 GPa
0.350 ksi
300% Modulus 0.00569 GPa
0.825 ksi
Tear Strength 41.2 kN/m
235 pli
Graves
Compression Set 72 %
72 %
Method B
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 142 °C
1.50 hour

@Temperature 287 °F
Users viewing this material also viewed the following: