Samyang Trimma® SD6320 PMMA, Translucent

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Samyang
Trade Name Trimma®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Samyang Trimma® SD6320 PMMA, Translucent.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 44.1 MPa
6400 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Yield Strength 49.0 MPa
7110 psi
ASTM D790
Flexural Modulus 1.62 GPa
235 ksi
ASTM D790
Izod Impact, Notched 1.47 J/cm

@Thickness 3.17 mm
2.76 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in