Material Notes:
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, wire and cable wrap, and industrial gasketing. PTFE = polytetrafluoroethyleneT-100 Skived Sheet and Film: PTFE sheet and film are manufactured from virgin PTFE resins which are molded, sintered, and skived to the appropriate thickness. Both sheet and film are widely used in a number of industries due to the material's outstanding characteristics, including heat and chemical resistance, dielectric strength, and anti-stick properties. Sheet and film may also be chemically etched on one or both sides for bondability.Virgin Skived Sheet: T-100 is a skived, virgin grade PTFE sheet. It is available in thicknesses ranging from 0.0115" to 0.25", and in widths of 12", 24", 36", and 48". PTFE film is supplied in either sheet or continuous roll form. Slit widths are available in thicknesses ranging from 0.001" to 0.062" and to the exacting tolerances of the wire and cable, and electronics industries. Custom colors are also available.Types of application include Electrical/Electronics, Medical, and Protective/DecorativeSpecification Notes: T-100 film meets the requirements of MIL-P-22241B, Type II, Grade A and other appropriate AMS and ASTM specifications.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D-792
Water Absorption <= 0.010 %
<= 0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 27.6 MPa
>= 4000 psi
ASTM D-882
Elongation at Break >= 300 %
>= 300 %
ASTM D-882
Tensile Modulus 0.552 GPa
80.0 ksi
ASTM D-882
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Melting Point 327 °C
620 °F
ASTM D-3418
Maximum Service Temperature, Air 260 °C
500 °F
UL-746 B
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 2.1

@Frequency 1000 Hz
2.1

@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 59.1 kV/mm
1500 kV/in
ASTM D-149
Dissipation Factor <= 0.00020

@Frequency 1000 Hz
<= 0.00020

@Frequency 1000 Hz
ASTM D-150