Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Nabaltec GmbH
Trade Name GRANALOX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nabaltec GRANALOX® NM 9915 B Ceramic Body, Binder Free.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nabaltec offers ceramic bodies with different alumina content as free-of-binder grades. With the addition of necessary amount of water (approx. 20 %) these grades can be directly used for slip casting. After the application of appropriate plasticizers they are also suitable for other molding technologies (e.g. extrusion, injection molding, tape casting).Information provided by Nabaltec.
Physical Properties Metric English Comments
Density 3.86 - 3.94 g/cc
0.139 - 0.142 lb/in³
Sintered
Moisture Absorption at Equilibrium <= 0.50 %
<= 0.50 %
Particle Size 160 - 220 µm
160 - 220 µm
Mean Granulate Size
Component Elements Properties Metric English Comments
Al2O3 99.7 %
99.7 %
Na2O 0.10 %
0.10 %
Processing Properties Metric English Comments
Sintering Temperature 1650 - 1750 °C
3000 - 3180 °F
Interval (dense ceramic parts)
1720 °C

@Time 7200 sec
3130 °F

@Time 2.00 hour