Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou POPTREEâ„¢ 6001A Flame-retarded Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer SPS Guang Zhou
Trade Name POPTREE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou POPTREEâ„¢ 6001A Flame-retarded Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristic: Low density, medium melt flow index, medium notched impact strength, no bloomingApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Flexural Strength 25.0 MPa
3630 psi
Flexural Modulus 1.10 GPa
160 ksi
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Flammability, UL94 V-2
V-2