Struktol STRUKSILON 8104 Silicone Stabilizer for PU Foam

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name STRUKSILON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol STRUKSILON 8104 Silicone Stabilizer for PU Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
STRUKSILON 8104 was developed as universal silicone stabilizer of medium potency for the production of conventional flexible polyurethane slabstock foam based on polyether polyols.Applications: STRUKSILON 8104 is applicable in systems for nearly all known flexible PU slabstock foam applications and technologies like production of seats, chairs, mattresses etc. in the furniture and automotive industry and for all kinds of damping devices.Information provided by Struktol
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Viscosity 825 cP

@Temperature 25.0 °C
825 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Optical Properties Metric English Comments
Refractive Index 1.4465

@Temperature 25.0 °C
1.4465

@Temperature 77.0 °F
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in closed original containers if transported and stored at temperatures between 1 and 30°C
Descriptive Properties Value Comments
Appearance Clear, colorless to slightly yellow liquid
Turbidity Point °C 29