Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufFlex™ GA-509-80-5 TPE Compound

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer S&E Specialty Polymers
Trade Name TufFlex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufFlex™ GA-509-80-5 TPE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Application: A Matte Finish, Flexible, Sunlight Resistant, 105?C Jacketing Compound with 60?C Oil Resistance.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 79.0

@Time 15.0 sec
79.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength >= 17.9 MPa
>= 2600 psi
ASTM D412
18.079 MPa

@Temperature 136 °C,
Time 605000 sec
2622.1 psi

@Temperature 277 °F,
Time 168 hour
Air Oven Aging
18.795 MPa

@Temperature 121 °C,
Time 605000 sec
2726.0 psi

@Temperature 250 °F,
Time 168 hour
Air Oven Aging
19.869 MPa

@Temperature 60.0 °C,
Time 605000 sec
2881.8 psi

@Temperature 140 °F,
Time 168 hour
Oil Immersion
Elongation at Break >= 350 %
>= 350 %
ASTM D412
238 %

@Treatment Temp. 60.0 °C,
Time 605000 sec
238 %

@Treatment Temp. 140 °F,
Time 168 hour
Oil Immersion
296.1 %

@Treatment Temp. 136 °C,
Time 605000 sec
296.1 %

@Treatment Temp. 277 °F,
Time 168 hour
Air Oven Aging
343 %

@Treatment Temp. 121 °C,
Time 605000 sec
343 %

@Treatment Temp. 250 °F,
Time 168 hour
Air Oven Aging
Thermal Properties Metric English Comments
Brittleness Temperature -21.0 °C
-5.80 °F
ASTM D746
Oxygen Index 26.0 %
26.0 %
ASTM D2863
Processing Properties Metric English Comments
Processing Temperature 171 - 182 °C
340 - 360 °F
Suggested Stock