Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills P6G2Z-090 Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Flint Hills P6G2Z-090 Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Excellent impact strength and weldability. Product does not contain animal derived components.Applications: Injection Molding and thermoforming - Automotive coolant bottlesInformation provided by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.3 g/10 min
1.3 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break >= 700 %
>= 700 %
ASTM D638
Tensile Modulus 1.17 GPa
170 ksi
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Gardner Impact >= 36.0 J

@Temperature -18.0 °C
>= 26.6 ft-lb

@Temperature -0.400 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
FDA 21 CFR 177.1520(c) 3.1