Material Notes:
Pa6 based unfilled GTX for Non-Auto marketThis data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D 792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
SABIC - Japan Method
Elongation at Break 100 %
100 %
SABIC - Japan Method
Flexural Strength 87.0 MPa
12600 psi
ASTM D 790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D 790
Izod Impact, Notched 6.37 J/cm

@Temperature 23.0 °C
11.9 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 75.0 - 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 - 47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 185 °C

@Thickness 3.20 mm
365 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D 257
Dielectric Constant 3.86

@Frequency 50.0 - 60.0 Hz
3.86

@Frequency 50.0 - 60.0 Hz
ASTM D 150