| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL NF1030 PPE+PS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.40 g/cc | 1.40 g/cc | ASTM D792 |
| Water Absorption | 0.060 % <br>@Time 86400 sec |
0.060 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0020 - 0.0030 cm/cm <br>@Thickness 3.20 mm |
0.0020 - 0.0030 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 120 | 120 | ASTM D785 |
| Tensile Strength, Yield | 108 MPa | 15700 psi | SABIC - Japan Method |
| Elongation at Break | 4.0 - 6.0 % | 4.0 - 6.0 % | SABIC - Japan Method |
| Flexural Strength | 140 MPa | 20300 psi | ASTM D790 |
| Flexural Modulus | 8.18 GPa | 1190 ksi | ASTM D790 |
| Izod Impact, Notched | 0.580 J/cm | 1.09 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 25.0 - 43.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
13.9 - 23.9 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 0.46 MPa (66 psi) | 128 °C <br>@Thickness 3.20 mm |
262 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |