SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.019 - 0.021 cm/cm

@Time 86400 sec
0.019 - 0.021 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.019 - 0.021 cm/cm

@Time 86400 sec
0.019 - 0.021 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527
Elongation at Break 100 %
100 %
ISO 527
Tensile Modulus 1.80 GPa
261 ksi
1 mm/min; ISO 527
Izod Impact, Notched (ISO) 44.0 kJ/m²

@Temperature 23.0 °C
20.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 96.0 kJ/m²

@Temperature 23.0 °C
45.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
124 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af