| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
| Density | 1.72 g/cc | 0.0621 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.480 % | 0.480 % | 50% RH, 24 hrs; ASTM D570 |
| 0.730 % | 0.730 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm @Time 86400 sec |
0.0030 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 240 MPa | 34800 psi | 5 mm/min; ISO 527 |
| 241 MPa | 35000 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 2.2 % | 2.2 % | 5 mm/min; ISO 527 |
| 2.4 % | 2.4 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 20.57 GPa | 2983 ksi | 1 mm/min; ISO 527 |
| 21.84 GPa | 3168 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 357 MPa | 51800 psi | ISO 178 |
| 371 MPa | 53800 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 17.9 GPa | 2600 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 18.12 GPa | 2628 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.53 J/cm | 2.87 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 12.5 J/cm | 23.4 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 75.0 kJ/m² | 35.7 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 10.0 J @Temperature 23.0 °C |
7.38 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Impact Test | 4.00 J | 2.95 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 19.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| CTE, linear, Transverse to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 253 °C @Thickness 3.20 mm |
487 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 237 °C | 459 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 240 °C @Thickness 3.20 mm |
464 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
UL 94 |