LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
1.57 g/cc
0.0567 lb/in³
ISO 1183
Moisture Absorption 0.830 %
0.830 %
50% RH, 24 hrs; ASTM D570
0.970 %
0.970 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 213 MPa
30900 psi
ASTM D638
214 MPa
31000 psi
ISO 527
Elongation at Break 2.8 %
2.8 %
ASTM D638
3.0 %
3.0 %
ISO 527
Tensile Modulus 17.09 GPa
2479 ksi
50 mm/min; ASTM D638
17.25 GPa
2502 ksi
1 mm/min; ISO 527
Flexural Strength 318 MPa
46100 psi
ISO 178
328 MPa
47600 psi
ASTM D790
Flexural Modulus 12.29 GPa
1783 ksi
ASTM D790
12.38 GPa
1796 ksi
ISO 178
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 94.0 kJ/m²
44.7 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 18.0 J
13.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 22.0 J
16.2 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
198 °C

@Thickness 3.20 mm
388 °F

@Thickness 0.126 in
unannealed; ASTM D648