Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 106 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 6.40 mm
223 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® MC8200 PC+ABS (Asia Pacific)
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
120°C/h; ISO 75/1
Polykemi AB POLYform POM C M140 TF2 Polyoxymethylene, Modified
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
120°C/h; ISO 75/1
Polykemi AB POLYform POM C M270 Polyoxymethylene
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Unannealed; ASTM D648
Multibase Nylex™ 2185 FR Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific)
Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior...
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ASTM D648
Gichem GILAC C120/T Acrylonitrile Butadiene Styrene  (discontinued **)
ABS with excellent thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 6.40 mm
223 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LG709W ABS, Low Gloss, Heat Resistance
Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
80x10x4mm; ISO 75-2/Af
SYNTHOS Forsan® 483 Acrylonitrile Butadiene Styrene (ABS)
High heat resistant, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Kau..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear (Europe-Africa-Middle East)
LNP* Lubricomp* OL004 is a compound based on PPS - Linear resin containing PTFE.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Unannealed; ASTM D648
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedTPCI# 7782121Information provided by T..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East)
Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat ..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Xylex X7509UV PC+POLYESTER (Asia Pacific)
PC+POLYESTER, Transparent, UV-Stabilized,This data was supplied by SABIC-IP for the Asia Pacific region.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 6.40 mm
223 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ISO 75
Styrolution Terluran® HH-106 ABS
Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Asia Pacific)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Asia Pacif..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 6.40 mm
223 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL CN1134 PPE+PS (Asia Pacific)
20% filled FR high modulus PPE/PS blend
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East)
EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ASTM D648
Denka MALECCA K-200 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided ..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 662 Nylon 6, Glass Bead Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
222 °F
Unannealed; ASTM D648
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific)
LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.