Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Spartech E65090 General Purpose PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Spartech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech E65090 General Purpose PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. Best for clear tubing, profiles and co-extrusion.Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
+.02
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
10 sec ± 3
Tensile Strength, Yield 20.4 MPa
2960 psi
Elongation at Break 320 %
320 %
100% Modulus 0.00752 GPa
1.09 ksi
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F