Material Notes:
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded into a wide variety of standard or custom isolators, including grommets, equipment mounts, bumpers, and gaskets. They feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.Information provided by Aearo E-A-R Specialty Composites.
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
5 sec.; ASTM D2240
Tensile Strength at Break 2.62 MPa
380 psi
ASTM D412
Elongation at Break 278 %
278 %
ASTM D412
Tensile Modulus 0.00134 GPa
0.195 ksi
ASTM D412
Compressive Yield Strength 0.100 MPa
14.5 psi
Compressive Load Deflection at 5%; ASTM D575
0.210 MPa
30.5 psi
Compressive Load Deflection at 10%; ASTM D575
0.320 MPa
46.4 psi
Compressive Load Deflection at 15%; ASTM D575
0.450 MPa
65.3 psi
Compressive Load Deflection at 20%; ASTM D575
0.620 MPa
89.9 psi
Compressive Load Deflection at 25%; ASTM D575
Compressive Modulus 0.00220 GPa
0.319 ksi
at 15% Compression; ASTM D575
Resilience 40
40
% Bashore Rebound; 22°C; ASTM D2632
53
53
% Bashore Rebound; 70°C; ASTM D2632
Tear Strength 10.2 kN/m
58.2 pli
ASTM D624
Compression Set 5.0 %
5.0 %
24 hour at 20°C; ASTM D395B
9.9 %
9.9 %
1/2 hour at 20°C; ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Continuous
125 °C
257 °F
Intermittent
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D2137
Flammability, UL94 HB
HB
Meets HBF
Descriptive Properties Value Comments
MVSS 302 Flammability Passes
Relative Peak Transmissibility 12.7 dB
G-411 Grommet; 1.2lb load @ 20°C