Material Notes:
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792A
Water Absorption 0.10 %
0.10 %
24 hours R.T. ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D651
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 16.0 GPa
2320 ksi
ASTM D790
Compressive Strength 200 MPa
29000 psi
ASTM D695
Izod Impact, Notched 0.578 J/cm
1.08 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C
>= 572 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 9.40 kV/mm
239 kV/in
Short Time; Dry; ASTM D149
Processing Properties Metric English Comments
Mold Temperature 155 - 180 °C
311 - 356 °F