Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SW83 Special High-Density Gunning Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chosun Refractories SW83 Special High-Density Gunning Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.69 g/cc
<br>@Temperature 1500 °C,<br> Time 10800 sec
0.0972 lb/in³
<br>@Temperature 2730 °F,<br> Time 3.00 hour
2.84 g/cc
<br>@Temperature 110 °C,<br> Time 86400 sec
0.103 lb/in³
<br>@Temperature 230 °F,<br> Time 24.0 hour
2.84 g/cc
<br>@Temperature 1000 °C,<br> Time 10800 sec
0.103 lb/in³
<br>@Temperature 1830 °F,<br> Time 3.00 hour
Porosity 20 %
<br>@Temperature 110 °C,<br> Time 86400 sec
20 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
20 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
20 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
22.5 %
<br>@Temperature 1500 °C,<br> Time 10800 sec
22.5 %
<br>@Temperature 2730 °F,<br> Time 3.00 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0024525 GPa
<br>@Temperature 110 °C,<br> Time 86400 sec
0.35571 ksi
<br>@Temperature 230 °F,<br> Time 24.0 hour
0.004905 GPa
<br>@Temperature 1500 °C,<br> Time 10800 sec
0.7114 ksi
<br>@Temperature 2730 °F,<br> Time 3.00 hour
0.005886 GPa
<br>@Temperature 1000 °C,<br> Time 10800 sec
0.8537 ksi
<br>@Temperature 1830 °F,<br> Time 3.00 hour
Thermal Properties Metric English Comments
Shrinkage -0.0500 %
<br>@Temperature 110 °C,<br> Time 86400 sec
-0.0500 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
-0.0500 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
-0.0500 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
2.0 %
<br>@Temperature 1500 °C,<br> Time 10800 sec
2.0 %
<br>@Temperature 2730 °F,<br> Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 83 %
83 %
SiO2 15 %
15 %
Descriptive Properties Value Comments
Main Applications Ladle