Material Notes:
Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EPDM, plasticized materials such as PVC and wood.Application: The CYNERGY SERIES of the cyanoacrylates should be applied in small amounts to one surface only. The parts should then be mated together under slight pressure. This causes the adhesive to spread out into a thin film and assures optimum adhesive performance. The pressure need only be applied for several seconds. The CYNERGY SERIES cures rapidly allowing for bonded parts to be handled within 10 to 60 seconds for most applications. Full cure is normally within 24 hours.Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Viscosity 1000 cP
1000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.3 MPa
2800 psi
Adhesive Bond Strength 29.0 MPa
4200 psi
Steel lap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time >= 0.133 min
>= 0.00222 hour
Fixture
480 min
8.00 hour
Full cure
Descriptive Properties Value Comments
Base Ethyl
Color Clear
Gap Fill (mil) 8