Mallard Creek Polymers Rovene® 4045 Styrene-Butadiene Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers Rovene® 4045 Styrene-Butadiene Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rovene® 4045 is recommended in applications where soil and aggregate stabilization and binding are required. Rovene® 4045 can be used in the process of road construction, landscaping, agriculture and erosion control applications. It provides good wetting of various soil types, imparts dry and wet strength to the soil and aggregates, and provides dust control.Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 4045 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 45 - 45.7 %
45 - 45.7 %
pH 7.8 - 8.4
7.8 - 8.4
Brookfield Viscosity <= 900 cP
<= 900 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 24.0 °C
75.2 °F
Descriptive Properties Value Comments
Emulsifiers Anionic