Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-functional UV-CC 2004 is a single component, solvent-less conformal-coating specifically formulated for rapid room temperature cure when exposed to UV light. Thin layer coatings cure almost instantly to a depth of 7 mils.UV-CC 2004 exhibits excellent adhesion to a variety of metals, ceramics and glass filled epoxy surfaces and is designed to meet the most demanding environmental needs of today’s PCB marketplace. This low viscosity coating can be cured by exposure to UV light and secondarily with heat for shadowed areas on densely populated circuit boards. UV-CC 2004 passes the “on-part” UL-94-V test.Processing: UV light cure: Bondline thickness of 7 mils; Exposure time of 5 seconds.Recommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Water Absorption 0.080 %
0.080 %
Viscosity 500 cP
500 cP
Nominal
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Elongation at Break 10 %
10 %
Thermal Properties Metric English Comments
CTE, linear 69.0 µm/m-°C

@Temperature 20.0 °C
38.3 µin/in-°F

@Temperature 68.0 °F
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Electrical Properties Metric English Comments
Volume Resistivity 3.50e+13 ohm-cm
3.50e+13 ohm-cm
Surface Resistance 3.70e+14 ohm
3.70e+14 ohm
Dielectric Constant 3.5

@Frequency 2.00e+9 Hz
3.5

@Frequency 2.00e+9 Hz
Dielectric Strength 66.9 kV/mm
1700 kV/in
Dissipation Factor 0.030

@Frequency 1e+6 Hz
0.030

@Frequency 1e+6 Hz
Descriptive Properties Value Comments
Color Clear Liquid
Cross Hatch Adhesion 1
Copper
100%
G-10