Reliance Industries Repol H050MN Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol H050MN Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
REPOL Polypropylene H050MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H050MN is recommended for injection molding and is an ideal choice as a compounding base and blending material in Furniture Compound. It is also suitable for molding Rigid Containers, Housewares and Thermowares. Repol H050MN contains Nucleating agent for high rigidity, reduced cycle time and Antistatic agent that reduces static charge build-up on products.Features:Low static charge buildup and reduced dust pickupConsistent processabilityExcellent color and processing stabilityInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 36.0 MPa
5220 psi
50mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50mm/min; ASTM D638
Flexural Modulus 1.75 GPa
254 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.350 J/cm

@Temperature 23.0 °C
0.656 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648