Radici Radiflam® A RV350AF (cond.) Nylon 66-35GF

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radiflam® A RV350AF (cond.) Nylon 66-35GF.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PA66 flame retardant injection molding grade with red phosphorus, halogen free. 35% Glass fiber reinforced, for items with high stiffness and good dimensional stability.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
Elongation at Break 2.2 %
2.2 %
Tensile Modulus 9.05 GPa
1310 ksi
Charpy Impact Unnotched 5.90 J/cm²

@Temperature -30.0 °C
28.1 ft-lb/in²

@Temperature -22.0 °F
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V