CMT Materials REN Shape® 470 Tooling Board, Modeling Board, Adhesive Products

Category Polymer
Manufacturer CMT Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMT Materials REN Shape® 470 Tooling Board, Modeling Board, Adhesive Products.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume production molds when forming in applications where metal molds do not makes sense due to time or cost considerations. CMT can help in selecting the proper board material for specific forming applications considering factors such as surface quality, ease in machining, tool durability, and forming temperature.Information Provided by CMT Materials, Inc.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0602 lb/in³
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
ASTM D-2240
Tensile Strength, Ultimate 32.4 MPa
4700 psi
ASTM D-638
Flexural Strength 60.0 MPa
8700 psi
ASTM D-790
Flexural Modulus 6.78 GPa
983 ksi
ASTM D-790
Compressive Strength 65.5 MPa
9500 psi
ASTM D-695
Compressive Modulus 5.97 GPa
866 ksi
ASTM D-695
Thermal Properties Metric English Comments
CTE, linear 40.9 µm/m-°C
22.7 µin/in-°F
ASTM D-3386
Glass Transition Temp, Tg 111 °C
232 °F
ASTM D-4065
Descriptive Properties Value Comments
Color Gray