| Category | Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), 30% Glass Fiber |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Duratron® PEI |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.51 g/cc | 1.51 g/cc | ASTM D792 |
| Water Absorption | 0.18 % | 0.18 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | 0.90 % | 0.90 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 114 | 114 | ASTM D785 |
| Hardness, Rockwell R | 127 | 127 | ASTM D785 |
| Hardness, Shore D | 86 | 86 | ASTM D2240 |
| Tensile Strength | 117 MPa | 17000 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Tensile Modulus | 5.52 GPa | 800 ksi | ASTM D638 |
| Flexural Strength | 186 MPa | 27000 psi | ASTM D790 |
| Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
| Compressive Strength | 221 MPa | 32000 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 4.31 GPa | 625 ksi | ASTM D695 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 Type A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 19.8 µm/m-°C <br>@Temperature -40.0 - 149 °C |
11.0 µin/in-°F <br>@Temperature -40.0 - 300 °F |
ASTM E831 |
| Thermal Conductivity | 0.225 W/m-K | 1.56 BTU-in/hr-ft²-°F | ASTM F433 |
| Maximum Service Temperature, Air | 171 °C | 340 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
| Glass Transition Temp, Tg | 210 °C | 410 °F | ASTM D3418 |
| Flammability, UL94 | V-0 | V-0 | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
| Dielectric Constant | 3.7 <br>@Frequency 1e+6 Hz |
3.7 <br>@Frequency 1e+6 Hz |
ASTM D150 |
| Dielectric Strength | 30.3 kV/mm | 770 kV/in | Short Term; ASTM D149 |
| Dissipation Factor | 0.0015 <br>@Frequency 1e+6 Hz |
0.0015 <br>@Frequency 1e+6 Hz |
ASTM D150 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Unacceptable | Unacceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Acceptable | Acceptable | |
| Hot Water / Steam | Acceptable | Acceptable | |
| Hydrocarbons - Aliphatic | Limited | Limited | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Unacceptable | Unacceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Machinability | 7 | 1-10, 1=Easier to Machine |