Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total Finathene® SI 508 HDPE blow molding  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finathene® SI 508 is part of a new generation of high density ethylene-hexene copolymers produced by the slurry loop low pressure polymerization process. Finathene® SI 508 is a high molecular weight pelletized resin intended for the blow-molding of medium size containers. Because of its high molecular weigh, Finathene SI508 may be used to produce containers with a higher impact strength, an excellent stress crack resistance and low creep under load. FINATHENE® SI 508 is best processed at temperatures between 180 and 220°C. FINATHENE® SI 508 has been especially developed for the production of containers to be submitted to the regulations for transportation of dangerous goods.Information provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D1693-70
High Load Melt Index 8.0 g/10 min

@Load 21.6 kg
8.0 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ISO 527
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527
Elongation at Break >= 700 %
>= 700 %
ISO 527
Elongation at Yield 9.0 %
9.0 %
ISO 527
Flexural Modulus 1.25 GPa
181 ksi
ISO 178
Tensile Impact Strength 110 kJ/m²
52.3 ft-lb/in²
Notched, -30°C; ISO 8256
230 kJ/m²
109 ft-lb/in²
Notched, 23°C; ISO 8256
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ISO 306
Descriptive Properties Value Comments
Food Approval This material complies with the main regulations concerning non-toxicity of plastics materials in contact with food stuffs.