A water-based coating designed to prevent molten metal adhesion to both refractory and most metallic surfaces. Multikote's bonding system enables it to be applied in a variety of applications including both hand and automatic ladles, thermocouple tubes, sow molds, troughs, casting tables, most boards, flooring, and other surfaces which require a protective coating. Stainless steel requires wire brush or acid prep.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Thermal Properties Metric English Comments
Melting Point -6.67 °C
20.0 °F
Maximum Service Temperature, Air 1649 °C
3000 °F