Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek M-2 Fiber Seal Pre-cut Gasket

Category Ceramic
Manufacturer Pyrotek, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek M-2 Fiber Seal Pre-cut Gasket.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A light-brown ceramic fiber material. Excellent trough gasket material.Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 0.0640 g/cc
0.00231 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1260 °C
2300 °F
Continuous
Users viewing this material also viewed the following: