Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamShine PV1003 ABS, General Purpose

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PV1003 ABS, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Water Absorption 0.30 %
0.30 %
DIN 53495
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Melt Flow 30 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM-D785
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM-D638
Elongation at Break 20 %
20 %
ASTM-D638
Izod Impact, Notched 2.60 J/cm

@Temperature 23.0 °C
4.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
DIN 53461
Vicat Softening Point 98.0 °C
208 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in