Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain relief's, and connectors. UL 94-V0 performance with good processability.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 173000 sec
0.10 %

@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0048 cm/cm

@Time 86400 sec
0.0048 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0109 cm/cm

@Time 86400 sec
0.0109 in/in

@Time 24.0 hour
ASTM D955
Melt Flow 31 g/10 min

@Load 5.00 kg,
Temperature 210 °C
31 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
33 g/10 min

@Load 2.16 kg,
Temperature 250 °C
33 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
30S reading; ASTM D2240
Tensile Strength at Break 10.0 MPa
1450 psi
Type I, 50 mm/min; ASTM D638
10.0 MPa
1450 psi
50 mm/min; ISO 527
Elongation at Break 115 %
115 %
50 mm/min; ISO 527
125 %
125 %
Type I, 50 mm/min; ASTM D638
Flexural Modulus 0.110 GPa
16.0 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.130 GPa
18.9 ksi
12.5 mm/min; ISO 178
Tear Strength 17.0 kN/m
97.0 pli
ISO 6383
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 5.00 mm
V-0

@Thickness 0.197 in
UL 94
Oxygen Index 25 %
25 %
ISO 4589
Glow Wire Test 800 °C
1470 °F
IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+15 ohm-cm
2.20e+15 ohm-cm
ASTM D257
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Smoke Density on 0.5mm plaque, Flame, Ds, max 90
ASTM E 662
Smoke Density on 0.5mm plaque, Non-flame, Ds, max 70
ASTM E 662