| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.35 g/cc | 0.0488 lb/in³ | DIN 53479 |
| Water Absorption | 5.8 % | 5.8 % | DIN 53495 |
| Moisture Absorption at Equilibrium | 1.8 % | 1.8 % | 50%RH; DIN 53714 |
| Linear Mold Shrinkage | 0.0080 - 0.010 cm/cm | 0.0080 - 0.010 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM-D638 |
| Elongation at Break | 4.0 % | 4.0 % | ASTM-D638 |
| Flexural Strength | 120 MPa | 17400 psi | ASTM D790 |
| Flexural Modulus | 3.60 GPa | 522 ksi | ASTM-D790 |
| Izod Impact, Notched | 0.500 J/cm <br>@Temperature 23.0 °C |
0.937 ft-lb/in <br>@Temperature 73.4 °F |
ASTM-D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 218 °C | 424 °F | |
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous Use |
| 180 °C | 356 °F | Short peaks operation | |
| Deflection Temperature at 0.46 MPa (66 psi) | 190 °C | 374 °F | DIN 53461 |
| Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C | 194 °F | DIN 53461 |
| Flammability, UL94 | HB <br>@Thickness 3.00 mm |
HB <br>@Thickness 0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | DIN 53482 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | DIN 53482 |
| Dielectric Constant | 3.8 <br>@Frequency 1e+6 Hz |
3.8 <br>@Frequency 1e+6 Hz |
VDE 0303/4 |