| Category | Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Synprene® RT-3850MS Styrene Butadiene Block Copolymer (SBC)
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.898 g/cc | 0.898 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 52 | 52 | ASTM D2240 |
| Tensile Strength at Break | 5.03 MPa | 730 psi | 510 mm/min; ASTM D412A |
| Tensile Strength, Yield | 2.93 MPa <br>@Strain 300 % |
425 psi <br>@Strain 300 % |
510 mm/min; ASTM D412A |
| Elongation at Break | 660 % | 660 % | 510 mm/min; ASTM D412A |
| Tear Strength | 26.3 kN/m | 150 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 20 % <br>@Temperature 23.0 °C,<br> Time 79200 sec |
20 % <br>@Temperature 73.4 °F,<br> Time 22.0 hour |
ASTM D395B |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | UV Stabilizer | |
| Appearance | Clear/Transparent | |
| Features | General Purpose | |
| Forms | Pellets | |
| Generic Name | Styrene Butadiene Block Copolymer (SBC) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Consumer Applications | |
| General Purpose |