Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Nymax™ 1308 A HS Black 13 Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Nymax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ 1308 A HS Black 13 Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 1.2 %

@Thickness 3.18 mm
1.2 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.016 cm/cm
0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.3 MPa
8600 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 45 %
45 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 1.50 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.81 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C

@Thickness 3.18 mm
144 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Appearance Black
Automotive Specifications CHRYSLER MS-DB41 CPN1826 Color: Black
Features General Purpose
Heat Stabilized
Impact Modified
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: