Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow INSPIRE™ TF1302 TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INSPIRE™ TF1302 TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medium Flow, High Impact, Filled TPOInformation provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line.
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ASTM D792B
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790A
Izod Impact, Notched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved