Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne LubriOne™ AS-000/15T Acrylonitrile Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer PolyOne Corporation
Trade Name LubriOne™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne LubriOne™ AS-000/15T Acrylonitrile Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.5 MPa
5000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 13 %
13 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1.38 GPa
200 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 79.3 MPa
11500 psi
ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 0.760 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.42 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C

@Thickness 3.18 mm
203 °F

@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 3.18 mm
185 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HB
HB
UL 94
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Processing Properties Metric English Comments
Mold Temperature 65.0 - 85.0 °C
149 - 185 °F
Drying Temperature 80.0 - 85.0 °C
176 - 185 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Features Lubricated
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
RoHS Compliance RoHS Compliant
Uses Appliance Components
Conveyor Parts
Printer Parts