| Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade | 
| Manufacturer | PolyOne Corporation | 
| Trade Name | Geon™ | 
| Port | Shanghai port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | PolyOne Geon™ Vinyl Wire & Cable WR7400L Polyvinyl Chloride, Flexible (PVC, Flexible).pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore A | 68 | 68 | 15 sec; ASTM D2240 | 
| Tensile Strength, Yield | 15.5 MPa | 2250 psi | Type IV, 510 mm/min; ASTM D638 | 
| Elongation at Break | 430 % | 430 % | Type IV, 510 mm/min; ASTM D638 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Maximum Service Temperature, Air | 105 °C | 221 °F | UL Temperature Rating | 
| Brittleness Temperature | -50.0 °C | -58.0 °F | ASTM D746 | 
| Oxygen Index | 24 % @Thickness 1.91 mm | 24 % @Thickness 0.0752 in | ASTM D2863 | 
| Processing Properties | Metric | English | Comments | 
|---|---|---|---|
| Melt Temperature | 155 - 165 °C | 311 - 329 °F | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Agency Ratings | UL QMTT2 | |
| Features | Flame Retardant | |
| Sunlight Resistant (720 hours) | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Extrusion Coating | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Retention of Tensile Elongation | 89% | 121°C, 1.91 mm; 500 hr, UL Standard | 
| Retention of Tensile Strength | 110% | 121°C, 1.91 mm; 500 hr, UL Standard | 
| RoHS Compliance | RoHS Compliant | |
| Uses | Cable Jacketing | |
| Flexible Cord Jacketing | ||
| Wire & Cable Applications | ||
| Wire Types | SJT | |
| SJTO |