Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade |
Manufacturer | PolyOne Corporation |
Trade Name | Geon™ |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | PolyOne Geon™ Vinyl Wire & Cable JAC31A Polyvinyl Chloride, Flexible (PVC, Flexible).pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.43 g/cc | 1.43 g/cc | ASTM D792 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 92 | 92 | 15 sec; ASTM D2240 |
Tensile Strength at Break | 20.7 MPa | 3000 psi | Type IV, 510 mm/min; ASTM D638 |
Elongation at Break | 290 % | 290 % | Type IV, 510 mm/min; ASTM D638 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 90.0 °C | 194 °F | UL Temperature Rating |
Brittleness Temperature | -28.0 °C | -18.4 °F | ASTM D746 |
Oxygen Index | 33 % @Thickness 1.91 mm |
33 % @Thickness 0.0752 in |
ASTM D2863 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 177 - 182 °C | 351 - 360 °F |
Descriptive Properties | Value | Comments |
---|---|---|
Additive | Lead Stabilizer | |
Agency Ratings | UL 444 | |
Features | Flame Retardant | |
Forms | Pellets | |
Generic Material | PVC, Flexible | |
Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
Processing Method | Extrusion Coating | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
North America | ||
South America | ||
Retention of Tensile Elongation | 80% | 121°C, 1.91 mm; 336 hr, UL Standard |
Retention of Tensile Strength | 100% | 121°C, 1.91 mm; 336 hr, UL Standard |
Uses | Communication Wire Jacketing | |
Wire & Cable Applications | ||
Wire Types | CL2 | |
CL2R | ||
CL3R | ||
CMR | ||
FPLR |