| Category | Polymer , Thermoplastic , Vinyl (PVC) |
| Manufacturer | PolyOne Corporation |
| Trade Name | Geon™ |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Geon™ Vinyl Flexible C70UB Polyvinyl Chloride, Flexible (PVC, Flexible).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.39 g/cc | 1.39 g/cc | ASTM D792 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 64 | 64 | 15 sec; ASTM D2240 |
| 70 | 70 | ASTM D2240 | |
| Tensile Strength at Break | 9.65 MPa | 1400 psi | Type IV, 510 mm/min; ASTM D638 |
| Tensile Strength | 4.34 MPa @Strain 100 % |
629 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
| Elongation at Break | 390 % | 390 % | Type IV, 510 mm/min; ASTM D638 |
| Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
| Compression Set | 20 % @Temperature 23.0 °C, Time 79200 sec |
20 % @Temperature 73.4 °F, Time 22.0 hour |
ASTM D395 |
| Clash Berg Modulus | 0.0814 GPa | 11.8 ksi | ASTM D1043 |
| 0.310 GPa @Temperature -46.0 °C |
45.0 ksi @Temperature -50.8 °F |
ASTM D1043 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Brittleness Temperature | -42.2 °C | -44.0 °F | ASTM D746 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 171 - 177 °C | 340 - 351 °F | |
| 193 - 199 °C | 379 - 390 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | Biocide | |
| UV Stabilizer | ||
| Features | Medium Gloss | |
| UV Absorbing | ||
| Forms | Pellets | |
| Generic Material | PVC, Flexible | |
| Generic Name | Polyvinyl Chloride, Flexible (PVC, Flexible) | |
| Processing Method | Coextrusion | |
| Extrusion | ||
| Injection Molding | ||
| Profile Extrusion | ||
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America |