Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical applications requiring high dielectric strength, low conductivity and corrosion resistance.Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 35% Filler by WeightAdditive:LubricantHeat Stabilizer Features: Antifreeze ResistantFatigue ResistantGasoline ResistanceGood Chemical ResistanceGood FlowHeat StabilizedHydrolysis ResistantLubricatedSolvent ResistantUses:Electrical/Electronic ApplicationsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Water Absorption 0.80 %
<br>@Time 86400 sec
0.80 %
<br>@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.6 %
1.6 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
<br>@Diameter 2.00 mm
0.0040 in/in
<br>@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
<br>@Diameter 2.00 mm
0.0090 in/in
<br>@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 153 MPa
22200 psi
ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 8.98 GPa
1300 ksi
ISO 527-2
Flexural Strength 189 MPa
27400 psi
ISO 178
Flexural Modulus 6.97 GPa
1010 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 180
14.0 kJ/m²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched 7.60 J/cm²
<br>@Temperature -30.0 °C
36.2 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
9.00 J/cm²
<br>@Temperature 23.0 °C
42.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
<br>@Temperature -30.0 °C
5.71 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
1.40 J/cm²
<br>@Temperature 23.0 °C
6.66 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Copyright © lookpolymers.com All Rights Reserved