Ascend Performance Materials Vydyne® 21FSR Nylon 66, General Purpose

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 21FSR Nylon 66, General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Vydyne® 21FSR is a high-viscosity, general-purpose PA66 resin. It is available in natural and designed for extrusion-compounding applications. This resin offers a well balanced combination of engineering properties characterized by high strength, rigidity, good toughness, high melt point, good surface lubricity and abrasion resistance. Vydyne 21FSR maintains the chemical resistance typical of PA66 to many chemicals, machine and motor oils, solvents and gasoline. Typical Applications/End Uses: CompoundingAvailability:Asia PacificEuropeNorth AmericaFeatures:Gasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood ToughnessHigh RigidityHigh StrengthLow Viscosity Oil ResistantSolvent ResistantUses:CompoundingGeneral PurposeAppearance: Natural ColorForms: PelletsProcessing Method: Compounding and Compounding ExtrusionInformation provided by Ascend
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Bulk Density 0.674 g/cc
0.0243 lb/in³
ASTM D1895
Relative Viscosity 48 - 54 cP
48 - 54 cP
ASTM D789
Viscosity Measurement 143 - 153
143 - 153
sulfuric acid; ISO 307
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357
Optical Properties Metric English Comments
Yellow Index 4.0 %
4.0 %
ASTM D1925
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
ASTM D789
Descriptive Properties Value Comments
RV, Formic Acid, ASTM D789 48-54