| Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergadur™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | PolyOne Bergadur™ PB400 G15 H UF UV Polybutylene Terephthalate (PBT).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0090 cm/cm | 0.0040 - 0.0090 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 78.5 MPa <br>@Temperature 23.0 °C |
11400 psi <br>@Temperature 73.4 °F |
ISO 527-2/5 |
| Flexural Strength | 156 MPa | 22600 psi | ISO 178 |
| Flexural Modulus | 6.60 GPa | 957 ksi | ISO 178 |
| Charpy Impact, Notched | 0.640 J/cm² <br>@Temperature 23.0 °C |
3.05 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 198 °C | 388 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | V-0 <br>@Thickness 0.800 mm |
V-0 <br>@Thickness 0.0315 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+14 ohm | 1.00e+14 ohm | ASTM D257 |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
| Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
| Drying Temperature | 110 - 120 °C | 230 - 248 °F | |
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | UV Stabilizer | |
| Appearance | Natural Color | |
| Features | Flame Retardant | |
| Halogen Free | ||
| Filler / Reinforcement | Glass Fiber Reinforcement, 15% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | PBT | |
| Generic Name | Polybutylene Terephthalate (PBT) | |
| Regional Availability | Asia Pacific |