Braskem EG0921 LDPE Blow Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem EG0921 LDPE Blow Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EG0921 is a low-density polyethylene with good mechanical properties and environmental stress cracking resistance (ESCR) and excellent sealability. It is used in blow molded parts and medium-resistance shrink films.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM-D1505
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM-D638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM-D638
Thermal Properties Metric English Comments
Vicat Softening Point 95.0 °C

@Load 1.02 kg
203 °F

@Load 2.25 lb
ASTM-D1525