Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® AS4C Carbon Fiber (3000 Filaments)

Category Carbon , Carbon Fiber , Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® AS4C Carbon Fiber (3000 Filaments).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Weight/length = 0.200 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin systems. They are used for weaving, braiding, filament winding applications, unidirectional tapes and prepreg tow for fiber placement. Chopped fibers are used in compression and injection molding compounds to produce machine parts, gears, and chemical valves. The finished products have excellent corrosion, creep and fatigue resistance plus high strength and stiffness characteristics.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 4150 MPa
602000 psi
Elongation at Break 1.8 %
1.8 %
Modulus of Elasticity 231 GPa
33500 ksi
Tensile modulus calculated at secant 6000-1000
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved