Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN®-N 055 SAN resin

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®-N
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN®-N 055 SAN resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These are typical values and are not intended for specification purposes. UL approved file No. is E142893. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Melt Flow 25 g/10 min

@Load 3.80 kg,
Temperature 230 °C
25 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D638
Flexural Yield Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm

@Thickness 3.17 mm
0.300 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
0.5 inch; ASTM D648
Flammability, UL94 HB
HB
UL94; UL approved File No. is E142893
Users viewing this material also viewed the following: