Greene Tweed WRâ„¢ 300 PEEK, Carbon Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Greene Tweed
Trade Name WR™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Greene Tweed WRâ„¢ 300 PEEK, Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
WR®300 is a carbon-fiber reinforced compression molded PEEK often selected by pump manufacturers and users for pump bushings and case or impeller wear rings. Maximum service life is achieved in clean, lubricated and/or moist environments.WR300 allows the pump user to increase pump efficiency by running tighter wear ring clearances while decreasing potential pump damage when pumps are cavitated or experience radial bearing failures.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 106
106
ASTM D785
Hardness, Shore D 93
93
ASTM D2240
Tensile Strength at Break 134 MPa
19400 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D1457
Tensile Modulus 10.8 GPa
1570 ksi
ASTM D638
Flexural Strength 212 MPa
30700 psi
ASTM D790
Flexural Modulus 10.9 GPa
1580 ksi
ASTM D790
Compressive Strength 202 MPa
29300 psi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 27.5 µm/m-°C

@Temperature 22.8 - 143 °C
15.3 µin/in-°F

@Temperature 73.0 - 290 °F
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
600 °F
Descriptive Properties Value Comments
Color Black