Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SHIELD® 4910 Conductive Coating

Category Polymer , Adhesive
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 4910 Conductive Coating.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Conductive CoatingInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Volatiles <= 15 %
<= 15 %
Component Elements Properties Metric English Comments
Silver, Ag 40 - 50 %
40 - 50 %
Descriptive Properties Value Comments
Acrylic Resin Proprietary wt. % Max 15
n-Butyl Acetate wt. % Max 15
Physical Form Gray liquid
Propylene glycol methyl ether acetate, wt. % 25-35
108-65-6
Talc wt. % Max 5